Firing temperature : cone 10 |
Surface texture : satin |
Color : brown |
Atmosphere:
Reduction
Ingredients
- 13.55
- 15.81
- 54.19
- 12.26
- 4.19
- 2.00
- 7.97
Add:
Instructions
This breaking glaze is beautiful for sculptural works, but isn't advised for contact with food.
This recipe was shared by Jennifer Higerd in the March 2019 issue of Ceramics Monthly.