Oatmeal Variation (1-B3-R9)
Firing temperature : cone 9 | Surface texture : matte to satin | Color : blue | Atmosphere: ReductionIngredients
- 5
- 20
- 50
Instructions
This recipe was sourced from The Ceramic Spectrum: A Simplified Approach to Glaze and Color Development by Robin Hopper.