Oak Ash

Oak Ash

Firing temperature : cone 9 | Surface texture : matte to satin | Color : brown | Atmosphere: Reduction Wood

Click Image to Enlarge

Instructions

I fire this glaze in reduction to cone 9 in the wood kiln. The oak ash is unwashed before use.

This recipe was shared by Jeff Diehl in the May 2020 issue of Ceramics Monthly.