Firing temperature : cone 6-10 | Surface texture : glossy to satin | Color : white | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

This glaze is very simple, reliable, great as a liner glaze, and also works for cone 10 reduction. It only runs when layered with a runny glaze. It works well with Mason stains for colors (I add 8% stain to the base). Omit the Zircopax for a great clear glaze.

This recipe was shared by Beth Bolgla in the June/July/August 2019 issue of Ceramics Monthly.