Firing temperature : cone 10 | Surface texture : matte to satin | Color : black | Atmosphere: Oxidation

This recipe was shared by Paul Ide in the February 2019 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

This semi-matte, cone 10 glaze also works well at cone 6. Do not use as a liner glaze.