Miranda Thomas Clear Transparent Glaze
Firing temperature : cone 9 | Surface texture : glossy | Color : clear | Atmosphere: OxidationIngredients
- 15
- 5
- 44
Instructions
Mix to a single cream consistency. This glaze works well over Miranda Thomas White Slip. Note: G200-EU Feldspar originates in Spain.
This recipe was shared by Miranda Thomas in the October 2020 issue of Ceramics Monthly.