Firing temperature : cone 10 | Surface texture : matte | Color : black | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

Allow slip to soak in water overnight before sieving to avoid lumps. Sieve through 80-mesh screen, then through a 100-mesh screen (do not screen through a 120-mesh screen). If too fine, it won’t adhere to the clay or glaze as well.

This recipe was shared by Miranda Thomas in the October 2020 issue of Ceramics Monthly.