Meer Flashing Slip
Firing temperature : cone 10-12 | Surface texture : glossy to satin | Color : Orange | Atmosphere: ReductionIngredients
- 33.3
- 33.3
- 33.4
Instructions
Dip pots into this slip or use a brush to apply. It works well on greenware or bisqueware.
This recipe was shared by Jacob Meer in the January 2020 issue of Ceramics Monthly.