Matte Flux Variation (1-B2-R9)
Firing temperature : cone 9 | Surface texture : glossy | Color : blue | Atmosphere: ReductionIngredients
- 12
- 17
- 35
- 17
- 12
Instructions
This recipe was sourced from The Ceramic Spectrum: A Simplified Approach to Glaze and Color Development by Robin Hopper.