Firing temperature : cone 10 | Surface texture : glossy | Color : medium purple | Atmosphere: Reduction

This is a glaze from Mark Talbert (Utah Valley University).

The test tile is Coleman Porcelain fired in reduction.


Click Image to Enlarge

Ingredients

Instructions

It will run if applied thickly.  For good color, reduce early.