Malcom Davis Carbon-Trap Shino

Malcom Davis Carbon-Trap Shino

Firing temperature : cone 10 | Surface texture : glossy | Color : medium orange | Atmosphere: Reduction

One of many carbon-trapping Shino recipes from Malcom Davis.

 


Click Image to Enlarge

Ingredients

Instructions

Reduce early and heavily for good carbon-trapping.