Malcolm Davis Shino Glaze
Firing temperature : cone 10 | Surface texture : matte | Color : black | Atmosphere: ReductionPublished in "Black Shino" by Mel Jacobson with Tom Buck, in the Dec 2000 issue of Ceramics Monthly.
Ingredients
- 17.27
- 9.82
- 40.91
- 18.18
Instructions
For use on porcelain, add 6% Cedar Heights Redart.