Firing temperature : cone 11 | Surface texture : matte to satin | Color : light brown | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Apply thick by dipping or pouring in and out if just used as liner. I fire this glaze to cone 11 in a wood kiln with heavy reduction. Fly ash in the firing can cause gray to pink speckling.

This recipe was shared by Scott McClellan in the October 2019 issue of Ceramics Monthly.