Firing temperature : cone 9-10 | Surface texture : matte | Color : gray | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Mix to a cream-like consistency and apply thickly by pouring or dipping. This glaze breaks on edges and throwing lines.