Lung Chuan Celadon for Reduction Cooling

Lung Chuan Celadon for Reduction Cooling

Firing temperature : cone 9-10 | Surface texture : glossy | Color : blue | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

This is one of the only fool-proof glazes I have found that works in reduction cooling. A beautiful blue celadon that brightens up and becomes more translucent around cone 10, and takes on the characteristics of a traditional semi-opaque, or milky celadon at cone 9.

This recipe was shared by Forrest Lesch-Middelton in the October 2020 issue of Ceramics Monthly.