Firing temperature : cone 03-04 | Surface texture : glossy | Color : blue | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Best when applied in a medium-thick application, equivalent to 3 pieces of construction paper stacked on top of one another.

This recipe was shared by Lisa Orr in the November 2019 issue of Ceramics Monthly.