Firing temperature : cone 10 | Surface texture : glossy | Color : clear | Atmosphere: Reduction

Published in "Mary Cay's Glittering Obsession" by Sumi von Dassow, in the Feb 2006 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Stains can be added to this glaze according to the manufacturer’s recommendations. For Yellow Glaze Kiln Jewels, 3% Cerdec yellow stain was added.

Carbonates and oxides also have been added to this recipe with success by using various proportions. A strong cobalt glaze was mixed with this glaze to produce the Sky Blue Glaze Kiln Jewel, but cobalt carbonate or oxide also could be used.

A wash of copper sulfate can be sprayed or brushed on to create the Copper Sulfate Glaze Kiln Jewels.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend