Firing temperature : cone 9-10 | Surface texture : crystalline | Color : blue | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

The glaze combination used on the pots in this photo is Crystalline Blue applied to the entire pot as the first glaze, followed by Lehman Blue applied to the top 80% of the exterior, followed by Trout applied to the top 65% of the exterior. The pieces were fired to cone 9–10 in reduction in a gas kiln.

This glaze is applied by dipping pots, and it works well layered in combination with other glazes. When used on its own, it is a glossy blue color.

This recipe was shared by Dick Lehman in the April 2020 issue of Ceramics Monthly.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend