Leach White

Leach White

Firing temperature : cone 10 | Surface texture : glossy | Color : white | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Ingredients

Instructions

I use this glaze on the rim of cups layered under San Miguel Icy Blue to create a watery, dripping effect.

This recipe was shared by Mark Chuck in the June/July/August 2019 issue of Ceramics Monthly.