Firing temperature : cone 10 | Surface texture : glossy | Color : light blue | Atmosphere:

Click Image to Enlarge

Ingredients

Instructions

This bluish-white glaze that is on the pot shown here is achievable only in cone-10 reduction soda firing. When used in other atmospheres, the fired result is a shiny white.

This recipe was shared by Olivia Tani in the March 2021 issue of Ceramics Monthly. 