Ceramic Recipes logo

Leach Temmoku

Leach Temmoku

Firing temperature : cone 10 | Surface texture : glossy | Color : clear | Atmosphere: Reduction

Published in "Celebrating Whiskey Bottles and Cups" by Matt Schiemann, in the Jul/Aug 2014 issue of Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Matt uses this glaze mainly as a liner for the interiors of his pots.