L6E

L6E

Firing temperature : cone 11 | Surface texture : satin matte | Color : dark brown | Atmosphere: Reduction

Published in "Lynn Lais" by Phyllis Blair Clark, in the Apr 2006 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

When applied thin, it is a dark brown; when applied light, it is a creamy oatmeal beige.