Kiln Wash

Kiln Wash

Firing temperature : Cone 07-10 | Atmosphere: Oxidation Reduction

Click Image to Enlarge

Instructions

For best results, I brush a thin coat on the interior of the soft-brick molds that I use to cast solid chunks of glaze. It also works well on kiln shelves.

This recipe was shared bu Alex Zablocki in the March 2020 issue of Ceramics Monthly.