Kilauea Red
Firing temperature : cone 10 | Surface texture : glossy | Color : red | Atmosphere: ReductionOriginally published in the February 2018 issue of Ceramics Monthly.
Ingredients
- 4.55
- 9.09
- 9.09
- 2.73
- 1.82
- 43.64
- 1.82
- 27.26
- 2.73
Add:
Instructions
Custer Feldspar can be used as the Potash Feldspar. An early reduction at 1800°F (982°C) will help the red to develop. It works best applied thick. On the vase above (1), Cortright applied the red glaze first, then waxed over it prior to applying the black glaze.