K-Shino

K-Shino

Firing temperature : cone 10 | Color : shino | Atmosphere: Reduction Wood

This glaze is a super versatile shino, beautiful on its own, or as a base glaze when layering.

Originally published in the December 2017 issue of Ceramics Monthly.


Click Image to Enlarge

Ingredients

Instructions

Rachel Clark uses this glaze primarily in a reduced wood firing but it will also do well in more oxizded regions of the kiln. It takes to oxide fusion printing quite well and seems to be compatible with a broad range of oxides.