JVM Orange

Firing temperature : cone 10 | Surface texture : satin | Color : Orange | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Mix the glaze to a half-and-half consistency. I use slip under JVM Orange to achieve a yellow color.