Firing temperature : cone 10 | Surface texture : glossy | Color : pink | Atmosphere: Reduction

This glaze is from Brian Jensen (Utah Valley University)

The test tile is Coleman Porcelain fired in reduction.


Click Image to Enlarge

Ingredients

Instructions

Because of the Erbium Oxide, the glaze color changes in different types of light.  (The glaze is pink in fluorescent light and blue in sunlight.)