Iron Ash

Iron Ash

Firing temperature : cone 10 | Surface texture : glossy to satin | Color : brown | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

This glaze is used as a liner only, because it is very runny! Apply thin by pouring. Firing to cone 10 in a wood kiln with heavy reduction. Fly ash from a wood firing can cause blue-gray streaky runs.

This recipe was shared by Scott McClellan in the October 2019 issue of Ceramics Monthly.