Interior Glaze for Flameware—Ann’s Kaki (Ann Stannard)

Interior Glaze for Flameware—Ann’s Kaki (Ann Stannard)

Firing temperature : cone 10 | Surface texture : matte | Color : medium brown | Atmosphere: Reduction

Only for use on lithium or cordierite bodies with very low coefficients of thermal expansion, and that have been fully tested as flameware. If used on other bodies, it will likely shiver off in sharp shards.

Published in "Flameware" by David Pier, in the May 2011 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Note: No guarantee is made by the author or CeramicRecipes.org regarding these recipes. All individuals must test materials and maintain quality control to ensure proper performance of any clay body - particularly flameware. To test if you actually have flameware after you fire it, don full protective clothing including a mask with a face shield and apply a propane torch flame directly to one spot on the test piece.  Once it gets red hot, pick it up with tongs and drop it in a metal bucket of water. If it can take that, then it is flameware. You still need to be careful because you can never be sure there aren't any pores that may create steam pressure in the future.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Share via
Send this to a friend