Honey Celadon

Firing temperature : cone 10 | Surface texture : matte | Color : golden yellow | Atmosphere: Reduction Soda Wood

Published in "Atmospheric Glazes" by Lisa York, in the Dec 2015 issue of Ceramics Monthly. The image shown here is the Honey Celadon glaze on top of Lisa York's Flashing Slip recipe. The orange-peeled grey areas in the image are just the Flashing Slip.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Do not apply thick or it may shiver or become runny.