Firing temperature : cone 10 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation/Neutral Reduction

Published in "Clear Liner Glaze" by Sam Chung, in the Nov 2014 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

Author note: After bisque firing the work to cone 06, I line the inside of the pot with this clear glaze. After firing to cone 10, I spray a cone 6 commercial clear glaze on the outside when the pot is still warm, which helps evaporate some of the water from the glaze. I reload it into an electric kiln and fire to cone 6. This may sound backward but it resolved a crazing issue I was having with my glaze.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend