Haynes Satin White Glaze
Firing temperature : cone 10 | Surface texture : satin matte | Color : white | Atmosphere: ReductionYields an opaque satin surface in soda firing, but can show the clay body texture.
Published in "Leaving the Nest" by Fred Herbst, in the Oct 2000 issue of Ceramics Monthly.