Hank’s Smooth Shino Glaze

Hank’s Smooth Shino Glaze

Firing temperature : cone 10 | Surface texture : satin matte | Color : white | Atmosphere: Reduction

White satin where thick; red where thin. Produces iridescence with oxides.

Published in "Shinos in the Fire...An Odyssey with a Doorless Fiber Kiln" by Hank Murrow, in the Sept 2001 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Best with early reduction and a long, concluding period of oxidation, or an oxidation soak during cooling.