Green/Maroon Glaze

Green/Maroon Glaze

Firing temperature : cone 10 | Color : dark red | Atmosphere: Oxidation/Neutral Reduction

Translucent green in reduction, maroon in oxidation.

Published in "Layers of Color" by Andrew Gilliatt, in the Jan/Feb 2011 issue of Pottery Making Illustrated.