Green to Black

Green to Black

Firing temperature : cone 10 | Surface texture : matte | Color : dark green | Atmosphere: Oxidation/Neutral Reduction

The glaze will be matt black when applied thick and soda fired in oxidation or reduction. A thin application combined with light soda glaze coverage can produce pumpkin oranges next to olive greens.

Published in "Working for Others or for Yourself, It's a Choice" by Dennis W. Smith with Ryan McKerley in the Mar 2006 issue of Ceramics Monthly.