Green Celadon

Firing temperature : cone 10 | Surface texture : glossy | Color : light green | Atmosphere: Reduction

Published in "Goblet with Elegance" by Yoshi Fujii, in the Jan/Feb 2015 issue of Pottery Making Illustrated.

Glossy green celadon breaks over texture.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Mix all dry ingredients together before adding water. Sieve through an 80-mesh screen to break up clumps and disperse colorants.