Ceramic Recipes logo

Glossy Cobalt Blue

Glossy Cobalt Blue

Firing temperature : cone 10 | Surface texture : glossy | Color : dark blue | Atmosphere: Oxidation/Neutral

This glaze is from Lasse Ostman, found on his website.

The test tile is Coleman Porcelain fired in oxidation.


Click Image to Enlarge

Ingredients

Instructions

This is a crystalline glaze and can be runny. Extreme care should be taken to protect shelves.