Forest Green Celadon

Forest Green Celadon

Firing temperature : cone 10 | Surface texture : matte | Color : dark green | Atmosphere: Reduction

Image shown is porcelain, Bisque Flash Slip, commercial underglaze, Forest Green Celadon, Shaner Clear Liner Glaze, soda fired to cone 10-11.

Published in "Soda Surfaces" by Nolan Baumgartner, in the Dec 2014 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments
  • Rick M.

    After a first series of tests, it seems this glaze runs seriously at cone 10+, cone 11 reduction. And this is on both Continental Clay domestic porcelain and Continental Clay Tableware stoneware. I will be doing more tests, and will post those results.

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend