Flat Matte Black
Firing temperature : cone 10 | Surface texture : matte | Color : black | Atmosphere: Oxidation/NeutralPublished in "Soft Slab Teapot" by Margaret Bohls, in the Mar/Apr 2010 issue of Pottery Making Illustrated.