Flashing Slip

Flashing Slip

Firing temperature : cone 10 | Surface texture : matte | Color : medium orange | Atmosphere: Reduction Salt Soda Wood

Published in "Atmospheric Glazes" by Lisa York, in the Dec 2015 issue of Ceramics Monthly. The image shown here is the Flashing Slip recipe on porcelain with Honey Celadon glaze over the Flashing Slip in some areas.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Mix to the consistency of very thick cream. Apply in a thin layer to leather-hard clay. Ball mill for 24 hours to break down the particle size of the Hawthorne Bond Fireclay.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image

Send this to a friend