Ceramic Recipes logo

Coleman’s Crab Claw Shino Glaze

Coleman’s Crab Claw Shino Glaze

Firing temperature : cone 10 | Surface texture : matte | Color : dark orange | Atmosphere: Reduction

This image shows the Coleman's Crab Claw Shino Glaze and mesquite ash sprinkled over the surface, fired to cone 10.

Published in "Tom and Elaine Coleman" by John Nance, in the Jan 2003 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

Yields a bright orange color, with a thin to medium application on porcelain. Dip or spray.