Coleman B’s Shino Glaze
Firing temperature : cone 10 | Surface texture : matte | Color : clear | Atmosphere: ReductionThis image shows Coleman B's Shino Glaze and dry mesquite ash fired to Cone 10 in reduction.
Published in "Tom & Elaine Coleman" by John Nance, in the Jan 2003 issue of Ceramics Monthly.
Ingredients
- 7
- 25
- 30
- 8
Instructions
A stiff surface glaze that will trap carbon if it is applied thickly and reduction is started around Cone 013.