Clear Glaze

Firing temperature : cone 10 | Surface texture : glossy | Color : clear | Atmosphere: Oxidation/Neutral Reduction

This recipe is courtesy of Northern Clay Center and was published in the February 2018 issue of Ceramics Monthly.


Click Image to Enlarge

Instructions

For Higgins’ work, she prefers to fire this recipe in reduction, but it does work in oxidation.