Bryce’s White Slip

Bryce’s White Slip

Firing temperature : cone 11 | Surface texture : matte | Color : white | Atmosphere: Oxidation/Neutral Reduction

Published in "Bryce Brisco: The Art of Serving" by Yoko Sekino-Bove, in the Mar/Apr 2014 issue of  Pottery Making Illustrated.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Bryce adjust the base recipe by adding varying amounts (between 2 and 10%) of Zircopax, Grolleg, feldspar, and/or silica to the bucket to change the opacity, whiteness, melt, and fit of the slip, respectively. This a a loose recipe for a bigportion, just like a home cooking recipe.

This item will be permanently deleted and cannot be recovered. Are you sure?

Once you submit this recipe for moderation you will no longer be able to edit its content.

Comments

Leave a Reply

You must be logged in to post a comment.

Enter Your Log In Credentials
This setting should only be used on your home or work computer.

Larger version of the image
Send this to a friend