Firing temperature : cone 10 | Surface texture : glossy | Color : medium brown | Atmosphere: Oxidation/Neutral Reduction

Published in "Letters" in the September 2012 issue of Ceramics Monthly.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

The addition of small percentages of iron oxide, rutile, or manganese dioxide will yield a varied palette of greens and browns.