Firing temperature : cone 10 | Surface texture : matte | Color : cream | Atmosphere: Reduction Soda Wood

Published in "Atmospheric Glazes" by Lisa York, in the Dec 2015 issue of Ceramics Monthly. The image shown here was fired in reduction in a wood/soda kiln to cone 10.


Click Image to Enlarge
Download for Glaze Calculation
Insight | Hyperglaze | Glaze Master

Ingredients

Instructions

Use hot water to dissolve soda ash when mixing to disperse the material and avoid clumping.