Firing temperature : cone 11 | Surface texture : glossy to satin | Color : blue | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Apply thick by dipping or pouring. Fire to cone 11 in a heavily reduced wood kiln to show off brushwork underneath the glaze. This glaze can become speckled and opaque where fly ash from a wood firing hits.

This recipe was shared by Scott McClellan in the October 2019 issue of Ceramics Monthly.