Ceramic Recipes logo

Black Wood Ash

Firing temperature : cone 10 | Surface texture : matte | Color : black | Atmosphere: Reduction

Click Image to Enlarge

Ingredients

Instructions

Use on exterior or non-food surfaces. This glaze yields a matte, lightly textured surface that begs to be handled. Mix a whole-milk consistency. This glaze is best applied by dipping. You may need to experiment with substituting some calcined EPK for EPK to ensure dry fit to your clay body.

This recipe was shared by Patrick Yeung in the December 2019 issue of Ceramics Monthly.