Base Ash Glaze
Firing temperature : cone 10 | Color : blue | Atmosphere: ReductionIngredients
- .3
- 33.4
- 16.2
- 25.9
- 24.2
- 1.1
- 0.8
For Blue Ash Glaze add:
Instructions
This glaze is a variation of others, and was developed further with my own experimentation. Wash, sieve, and dry the ash prior to adding it to the recipe. I use this glaze above Temple Black, which is applied to the lower section of the pot.
This recipe was shared by Seth Guzovsky in the January/February 2020 issue of Pottery Making Illustrated.