Ash Glaze

Ash Glaze

Firing temperature : cone 10-14 | Surface texture : glossy | Color : dark brown | Atmosphere: Oxidation/Neutral Reduction

This recipe was originally published in the January/February 2018 issue of Pottery Making Illustrated.


Click Image to Enlarge

Ingredients

Instructions

This recipe is best applied to leather-hard clay. *I collect wood ash from our wood stove and wash and sieve the ash through a window screen. **I use glass beads sourced from a local sandblasting supply shop.